Home /

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products

Send your message to this supplier
*From:
Your email address is incorrect!
To:Eternal Bliss Alloy Casting & Forging Co.,LTD.
*Subject:
Your subject must be between 10-255 characters!
*Message:
Your message must be between 20-3,000 characters!
Yes!I would like your verified suppliers matching service!
Buy cheap Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products from wholesalers
  • Buy cheap Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products from wholesalers
  • Buy cheap Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products from wholesalers
  • Buy cheap Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products from wholesalers
  • Buy cheap Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products from wholesalers
  • Buy cheap Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products from wholesalers
  • Buy cheap Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products from wholesalers

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products

Ask Latest Price
Brand Name:Eternal Bliss
Model Number:EB26078
Certification:ISO9001-2008
Price:USD80/kg ~ USD120/kg
Payment Terms:by T/T or L/C, Western Union
Supply Ability:100,000,000.00
Delivery Time:It depends on the quantity to be ordered.
Company Data
Active Member
Contact Person Juliet Zhu
Business Type: Manufacturer Distributor/Wholesaler Agent Importer Exporter Trading Company Seller
Officials: 1099 Xinhua Road,214104, Xishan District, Wuxi, Jiangsu,China
Quality: Quality Certifitation Available
Visit Website
Product Details Company Profile
Product Details

Precision Cast Process X-40 Cobalt High Speed Steel Products with High Accuracy EB26078

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products.


Precision investment casting services for a variety of high temperature super alloys cobalt-based types.

Provides on-site engineering support, tooling design, surface treatment, laboratory testing, and warehousing services. Just in time delivery and other logistics services are available.


We produce High Temperature Superalloy Castings Parts with precision investment process.


Table 1 : Standard Cobalt cobalt alloy Alloy

CoCrCWMoNiSiBFeMnOthers
cobalt alloy 1BAL332.4513-2.5*1-2.5*1-
cobalt alloy 3BAL312.513-2.5*1-2.5*1-
cobalt alloy 4BAL31.5114-2.0*1-2.0*1-
BAL281.25-3.0*1-2.5*1-
cobalt alloy 12BAL291.859-2.5*1-2.5*1-
cobalt alloy 20BAL332.4517.5-2.5*1-2.5*1-
cobalt alloy 21BAL270.25-5.52.5*1-3.0*1-
cobalt alloy 31BAL260.57.5-10.51-2.0*1-
cobalt alloy 190BAL263.314-1.01-8.00.5-
cobalt alloy 238BAL260.1-3-1-20.01-
cobalt alloy 306BAL250.42-6.01-4.0*1Nb=5
94BAL28119-5.01-2.5*1V=1
cobalt alloy FBAL25.51.7512.25-22.51-1.5*--
cobalt alloy SF1BAL191.313-1332.53*0.5Cu=0.5
cobalt alloy SF6BAL190.77-132.51.73*0.5Cu=0.5
cobalt alloy SF12BAL1919-13323*0.5Cu=0.5
cobalt alloy SF20BAL191.515-13332*0.5Cu=0.5
TRIBALOY T400BAL80.1*-283*2.4-3*--
TRIBALOY T800BAL170.1*-283*3.2-3*--
DELORO 15--0.06*--BAL2.01.051.5*20Cu=20
DELORO 22-0.700.10--BAL2.31.75---
DELORO 40-7.00.10--BAL3.52.25---
DELORO 50-10.250.45--BAL4.01.854.0--
DELORO 60-14.250.6--BAL2.03.54.0--
DELORO 625-220.1-9BAL--5--
NISTELLE C-16.50.12*4.517BAL0.7-6.0--
TRIBALOY T700-150.10*-32BAL3.25-
Hastelloy C22®(UNS N06022)(Max.)
CMNPSSiCrNiMoCOFeWV
0.0150.50.020.020.0820.0-22.5Bal.12.5-14.52.52.0-6.02.5-3.50.35
Hastelloy C276®(UNS N10276)(Max.)
CMNPSSiCrNiMoCOFeWV
0.0110.040.030.0814.5-16.5Bal.15.0-17.02.54.0-7.03.0-4.50.35
Hastelloyx®(UNS N06002)(Max.)
CMNPSSiCrNiMoCOFeWother
0.05-0.1510.040.03120.5-23.0Bal.8.0-10.00.5-2.517.0-20.00.2-1.0/
Monel 400®(UNS NO4400) (Max.)Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
CMNSSiNiCuFe
0.320.0240.563 min28-342.5
Monel M400®(UNS NO4400)(Max.)Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
CMNSSiNiCuFe
0.320.0240.563-7028-342.5
Monel R405®(UNS NO4405)(Max.)Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
CMNSSiNiCuFe
0.320.025-0.060.563.0min28-342.5
Monel K500®(UNS NO5500)(Max.)Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products
CMNSSiNiCuTiAIFe
0.120.010.563min27-330.862.3-3.152
Inconel 600(UNS NO6600)(Max.)
CMNSSiCrNiCuFe
0.1510.0150.514-1772 min0.56.0-10.0
Inconel 601(UNS NO6601)(Max.)
CMNSiCrNiCOAIFe
0.050.30.222.561.5min51.414.1
Inconel 718(UNS NO7718)(Max.)
CrNiMoCOCb+TaTiAIFe
1952.5min3.0555.130.90.518.5
Chemical Analysis of Incoloy 800® uns(N08800)
CCrNiTiAIFeGrain
0.1 max19.0-23.030.0-35.00.15-0.60.15-0.639.5min/
Incoloy800H® UNS(N08810)
CCrNiTiAIFeGrain
0.05-0.119.0-23.030.0-35.00.15-0.600.15-0.6039.5min5or coarser
Incoloy800HT® UNS(N08811)
CCrNiTiAIFeGrain
0.06-0.1019.0-23.030.0-35.00.25-0.600.25-0.6039.5min5or coarser

Dimensions:as per drawings


Production Process

Step 1: Getting orders.


Step 2: Process design by technical department


Step 3: Purchase of raw materials and pattern making &checking


Step 4: Inspection of raw materials


Step 5: Melting by middle-frequency induction furnaces


Step 6: Ladle analysis by Spectrometer


Step 7: De-oxidization, slag-removal, tapping


Step 8: Pouring


Step 9: Openning & fettling


Step 10: Surface & dimensional check


Step 11: Heat treatment


Step 12: Inspection of physical property (UT test,MT test, hardness,impact value µstructure)


Step 13: Packing


Step 14: Shipping


Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products

1. 16-year Foundry Operation Experience.

2. Friendly & High Efficient Technical & Commercial Communication.

3. Professional Export Practices: Have Exported to +60 Overseas Countries.



Our Trade Show Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products


Our booth No. 14-A29-5 in Newcast 2015,Germany

Hall 14, Stand No.A29-5.


Contact Us for further information about products & service:

Mr.John Liu

Project Manager

Cell: 0086-130 930 23772(What's App)

Tel: 0086-188 0059 6372

Fax: 0086-510-6879 2172

E-mail: cast@ebcasting.com; ebcastings@163.com

Skype ID:julia.zhu26

QQ: 217 039 6403

Precision Superalloy Castings Parts X-40 Cobalt High Speed Steel Products www.ebcastings.com


Eternal Bliss Alloy Casting & Forging Co.,LTD.
Company Profile

Eternal Bliss Alloy Casting & Forging Co.,LTD.

EB China makes metal better.

EB China is a professional manufacturer of high alloy castings and forgings with 22-year history!!Our main products include corrosion, wear & heat-resistant castings & forgings.

Our foundry & forging plant have passed ISO9001,ISO14001,ISO45001 Management System Certification and one whole set of inspection report will be submitted for your approval before shipment.

The registered capital of EB China is CNY13.14 million.

Three shops on Alibaba.TUV and SGS come to us to do onsite assessment every year.

Total online revenue is more than USD4 million.

22 Techncial Patents.EB China has achieved GB/T 29490-2013 Interllectual Property Management System Certification.

5 Trade Marks

We EB China have been listed into Jiangsu Province High New Technologicl Enterprise Database.

Our high alloy castings & forgings have been exported to over 69 overseas countries.

We can supply high efficient service:

We can provide 24-hour service hotline: 0086-130 930 23772(what's app)

We are the director member of Wuxi E-commerce Chamber and the Vice President of Wuxi Lianyungang Commerce Chamber.

Our mission is LET'S CAST THE SOUL INTO OUR PARTS TO ACHIEVE THE BEAUTY OF INDUSTRY.

We sincerely hope that we can use our metallurgical and material expertise to be at your service.

My dear friend, if you need any high alloy castings and forgings, please surely send us your inquiry to cast@ebcastings.com! Thank you.

Send your message to this supplier
*From:
Your email address is incorrect!
*To:

Eternal Bliss Alloy Casting & Forging Co.,LTD.

*Subject:
Your subject must be between 10-255 characters!
*Message:
Your message must be between 20-3,000 characters!
Characters Remaining : (0/3000)

You May Like

China Corrosion - Resistant Bearing Precision cobalt alloy Bushing Of Cobalt Alloy wholesale

Corrosion - Resistant Bearing Precision cobalt alloy Bushing Of Cobalt Alloy

China X-40 Cobalt Alloy Castings Parts Temperature Up to 1300 Degree EB9110 wholesale

X-40 Cobalt Alloy Castings Parts Temperature Up to 1300 Degree EB9110

China Cobalt Forgings 3mm Thick Coating 316L Customized Forging Adapter Parts ASTM A297 HP EB3386 wholesale

Cobalt Forgings 3mm Thick Coating 316L Customized Forging Adapter Parts ASTM A297 HP EB3386

China ASTM F799-11 Cobalt Base Alloy for Surgical Operation Cast with Forging Process EB3388 wholesale

ASTM F799-11 Cobalt Base Alloy for Surgical Operation Cast with Forging Process EB3388

China Elastic Cobalt Alloy Castings SOFC Sealing Material Shot Blast Surface Treatment wholesale

Elastic Cobalt Alloy Castings SOFC Sealing Material Shot Blast Surface Treatment

China  Coating 3mm Thick Open Die Forging / Adapter Component Wear Resistant wholesale

Coating 3mm Thick Open Die Forging / Adapter Component Wear Resistant

China ISO 9001 Certification Cobalt Alloy Castings High Temperature Investment Cast Process wholesale

ISO 9001 Certification Cobalt Alloy Castings High Temperature Investment Cast Process

China X-40 Cobalt Alloy Castings Anti Corrosion With Precision Cast Process EB26079 wholesale

X-40 Cobalt Alloy Castings Anti Corrosion With Precision Cast Process EB26079

China Chromium - 6 Cobalt - 28 / Molybdenum Alloy Castings For Surgical Implants wholesale

Chromium - 6 Cobalt - 28 / Molybdenum Alloy Castings For Surgical Implants

China EB Investment Cobalt Chrome Lost Wax Casting Australian Metal Parts wholesale

EB Investment Cobalt Chrome Lost Wax Casting Australian Metal Parts

China Crack Resistant Cobalt Alloy Bushings And Sleeves Wear Corrosion Resistant wholesale

Crack Resistant Cobalt Alloy Bushings And Sleeves Wear Corrosion Resistant

Inquiry Cart 0